Susbaint ceimigeach,%
Ni | Mn | Fe | Si | Cu | Eile | Stiùireadh RoS | |||
Cd | Pb | Hg | Cr | ||||||
2 ~ 5 | 11 ~ 13 | <0.5 | micro | Bal | - | ND | ND | ND | ND |
Togalaichean meacanaigeach
Temp seirbheis leantainneach Max | 0-100ºC |
Cuibheasachd aig 20ºC | 0.43 ± 0.04ohm mm2 / m |
Dùmhlachd | 8.4 G / CM3 |
Euctionality Thermal | 40 kJ / m · h · ºC |
Co-èifeachd Temp an aghaidh 20 ºC | 0 ~ 40α × 10-6 / ºC |
Puing leaghaidh | 1450ºC |
Neart tensile (HARD) | 585 MPA (Min) |
Neart tensile, n / mm2 Baigheil, bog | 390-535 |
Elong | 6 ~ 15% |
EMF VS Cu, μv / ºC (0 ~ 100ºC) | 2 (Max) |
Structar icrocorra | Austenite |
Seilbh Magnetach | neo- |
Cruas | 200-260hb |
Structar icrocorra | Ferrite |
Seilbh Magnetach | Magnetic |