1.CeimigeachCco-chur
| Stuth | Co-dhèanamh ceimigeach (%) | ||||
| Ni | Cr | Si | Mn | Al | |
| KP (Cromel) | 90 | 10 | |||
| KN (Aluminium) | 95 | 1-2 | 0.5-1.5 | 1-1.5 | |
2.Feartan corporraagus feartan meacanaigeach
| Stuth | Dlùths (g/cm3) | Puing leaghaidh ℃) | Neart teannachaidh (Mpa) | Frith-sheasmhachd toirte (μΩ.cm) | Ìre sìneadh (%) |
| KP (Cromel) | 8.5 | 1427 | >490 | 70.6 (20℃) | >10 |
| KN (Aluminium) | 8.6 | 1399 | >390 | 29.4 (20℃) | >15 |
3.Raon luach EMF aig teòthachd eadar-dhealaichte
| Stuth | Luach EMF an aghaidh Pt(μV) | |||||
| 100℃ | 200℃ | 300℃ | 400℃ | 500℃ | 600℃ | |
| KP (Cromel) | 2816~2896 | 5938~6018 | 9298~9378 | 12729~12821 | 16156~16266 | 19532~19676 |
| KN (Aluminium) | 1218~1262 | 2140~2180 | 2849~2893 | 3600~3644 | 4403~4463 | 5271~5331 |
| Luach EMF an aghaidh Pt(μV) | ||||
| 700℃ | 800℃ | 900℃ | 1000℃ | 1100℃ |
| 22845~22999 | 26064~26246 | 29223~29411 | 32313~32525 | 35336~35548 |
| 6167~6247 | 7080~7160 | 7959~8059 | 8807~8907 | 9617~9737 |
SEÒRSA K (CROMEL an aghaidh ALUMEL)air a chleachdadh ann an àilean ocsaideachaidh, neo-ghnìomhach no lughdachadh tioram. Tha nochdadh do fhalamh air a chuingealachadh ri ùine ghoirid. Feumar a dhìon bho àilean sulfarach agus àilean a tha beagan ocsaideachaidh. Earbsach agus ceart aig teòthachd àrd.